Contents
Purification
....
Restriction
...
GA
...
Soft lithography - PDMS molding
- Silicon masters
- 40g PDMS + 4g curing agent
- curing 80°C/2h
Soft lithography - Bonding PDMS-Glass
Preparation of the substrates
Glass slide
- 2.5 minutes air plasma treatment
PDMS
- Cut the PDMS
Air plasma treatment
- Position the substrate
Permanent irreversible bonding
- Place PDMS over glass slide
- post-bake 80°C/1h
...